Skip to content
64 pieces, each one of onePrices in USD
All piecesLiddedON-E-01USD $248
Lidded Box 300, piece ON-E-01, woven in Rattan. This is the piece you would receive.1 of 1 — the photograph is this piece

ON-E-01 · Lidded

Lidded Box 300

plant fibreRattan24 h at the weave · weaver W-01

Split climbing-palm cane. Soaked, then bent while wet. Unprocessed plant material.

Measured +9 mm against the drawing at mouth diameter (widest point). All three measured points are below, along with the flaw you can see in the photographs.

Where this one can go

This is a plant-fibre piece. Some countries will not take it, and some need a certificate. Pick your country and we will tell you which applies before you buy.

Not sent to: AU · NZ · full list

USD $248One piece, then gone

Shipping is added at checkout. Import duties and taxes raised by your own country are not included and are yours to pay. Hong Kong charges no sales tax on this sale.

Thirty days to change your mind — our promise, and it does not cut down any statutory right you have where you live. Returns · Delivery

+9mouth diameter300309 mm+7base diameter240247 mm+4height240244 mmON-E-01 · RATTANFRONT ELEVATION · ONE SCALE FOR BOTH OUTLINES
Dashed — the drawingSolid — this pieceHatched — the difference. Both outlines at one scale.

Against the drawing

Measured with a digital calliper forty-eight hours after the weaving finished, at 22 °C and 50–60% relative humidity. Natural fibre moves with humidity; the same piece read in a damp room measures larger.

ON-E-01 — measured against the drawing, in millimetres
PointDrawingThis pieceDifference
Mouth diameter (widest point)300309+9 mm
Height (excluding handle)240244+4 mm
Base diameter240247+7 mm

We do not grade pieces by how close they came, and this one costs exactly what its opposite number costs. Why

This piece, close up

The weave and rim of ON-E-01 in close-up. Body woven up from a six-point base; the lid is worked separately and closes at the front.
The weave, and where it starts
The visible flaw on ON-E-01: The lid sits 3 mm proud at the back when closed. A cane has split for 7 mm on the body wall near the front.
The flaw, not retouched
ON-E-01 photographed beside a ruler so you can judge its size against the published 309 mm.
Against a ruler

What was hand work

Seven steps — which were hand work on this piece
StepWhat it coversOn this piece
Preparing the fibreSplitting, soaking, scraping to thicknessBy hand
The weaving itselfThe body of the pieceBy hand
Rim and edgeBinding, borders, closing offBy hand
ColourWhether anything was added to the fibreNone
SurfaceWax, seal or nothing at allNone
HardwareAny bought-in metal or fittingNone
Base or standAny bought-in structural partNone

The weaving is hand work on every piece here — that is the premise of the shop. The other six steps vary, and we say which is which rather than calling the whole thing handmade. Where we draw the line

Four things that belong to this one only

Where the weave runs
Body woven up from a six-point base; the lid is worked separately and closes at the front.
How the colour falls
The lid is a half-tone lighter than the body — it was woven from the tail of the earlier bundle.
What you can see wrong with it
The lid sits 3 mm proud at the back when closed. A cane has split for 7 mm on the body wall near the front.
Woven by
W-01 — a code, not a name. We do not publish the names of the people who weave for us.

Numbers and limits

Carrying load
7 kg
Lifted by the rim or handle. The handle fails first, so this is the lower figure.
Recorded weaving time
24 h
The weaving only. Preparing and drying the fibre are not counted.
Outer carton
400 × 400 × 340 mm
Large parcel. Shipping is charged on volumetric weight.

Not made for children, not made for direct contact with food, and not made to carry structural load or to be sat or stood on.

What this material does over time

The long version →
Cracking
Rattan and bamboo lose water in a heated or air-conditioned room and split. Keep the room between 40% and 65% relative humidity.
Deforming
Loaded or hung for long enough, a woven wall dishes and a rim pulls out of round. The carrying figure below is the figure, not a suggestion.
Darkening
Undyed fibre in daylight turns deeper and greyer. That is oxidation and it does not reverse.
Mould
Above about 75% relative humidity, natural fibre grows mould. Dry it, brush it, and treat it early.
Insects
Plant fibre can be bored by insects. We do not claim any piece is proof against them.
Burrs and broken strands
Strands lift and break with use. Trim a burr flush and splice a break with repair cord.